Luperox® JWEB™ 50 polymer initiator

Product

Luperox® JWEB™ 50 polymer initiator structure can assist in production of polystyrenes with  long-chain branching, which may be difficult to achieve with traditional initiators.

1 hour half-life temperature in ethyl benzene: 119.2°C

 

Available formulations:

  • Luperox® JWEB50: 50% active weight in ethyl benzene solvent